1. TPU: Lub qhov kub kub nyob ntawm lub hardness. Rau 60A-80A, siv 90-100 degree; rau 85A-98A, siv 100-105 degree; Rau 60D-71D, siv 105-110℃rau 3-5 teev.
2. LCP: Qhov ci thiab moulding kub sib txawv ntawm cov neeg tsim khoom sib txawv. Piv txwv li, lub EI series los ntawm polyclastics Japer yog tsim rau maub ntawm 340-370 degree, nrog ib qho kev txwv sab sauv ntawm 365℃rau tsis tshaj 30 feeb.
3. PA cov khoom lag luam: ib lub crystalline thermoplastic nrog qhov sib txawv yaj yaj. Nylon 6 muaj ib qho tm ntawm 220-230 degree, thaum Nylon 66 muaj ib qho TM ntawm 260-270 degree. Nylon yog xam phaj hygroscopic thiab yog li ntawd yuav tsum tau kom qhuav ua ntej molding. Kom qhuav ntawm kev kub siab dhau ib qho kub yuav ua rau tsis txaus ntseeg ntawm cov nylon pellets.
4. PC / ABS Yas Khoom siv feem ntau muaj lub ntiajteb txawj nqus tshwj xeeb ntawm 0.2%, ib qho kev ua pa dej ntawm 0.4-6, thiab cua sov distortion kub ntawm 120%. Lub tshuab ziab khaub ncaws kom qhuav yuav tsum muaj 100 degree, thiab cov khoom yuav tsum tau ci ntawm qhov kub ntawm 100-110℃rau 3-4 teev.
5. Raws li: Nozzle tea: 190-210 degree, kev tshuaj ntsuam siab: 5-30 degree, rov qab ntsuas kub: 80-100 lub sijhawm ci: 2-4 teev.
6. PBT cov khoom siv yas: Nozzle kub: 230-245 degree, tuav siab: 5-10 degree: 100-140 degree: 4-6 teev.
7 Tus Tsiaj: Nozzle 240-270℃F, Kev Kho F, Ntsig Kub Siab F, Ntsia Ris Kub 100-140 Degree F, Lub Sijhawm Kho Mob 6-8 teev.
8 PC cov khoom siv: Nozzle 270-300 Degree F, Pwm Kub 80-120 Degree F, Kho Sij Hawm Kub 100-120 Degree Sijhawm 2-4 teev.
9 PA6: Nozzle 250-260℃f, pwm kub 50-110℃f, kho qhov kub 80-110 sijhawm sijhawm 4-6 teev.
10 pa66 Yas Khoom Siv: Nozzle 250-280 Degree F, Pwm Kub 50-110 Degree F, Qhov Ntsuas Kub 80-130 Lub sij hawm 4-6 teev.
11. PPS Cov Khoom Siv Yas: Nozzle kub 290-300 Degree, pwm kub 80-150 degree, ci kub 120-140 degree, ci sij hawm 2-4 teev.
12. LCP: Nozzle kub 3500-310 degree, pwm kub 90-180 degree, ci kub 130-140 degree: ci sij hawm 2-4 teev.
13. Dupont pom cov khoom siv yas no: Nozzle kub 170-230 degree, pwm kub 50-80 degree, ci kub li 2-120 degree, ci sij hawm 2-4 teev.
14. PP: Nozzle sov 200-220 degree, pwm, ua kom sov li ntawm 40-60 degree, ci℃80-120℃lub sijhawm 2-4 teev.
15. PPO: Nozzle kub 210-260 degree, pwm kub 50-90 degree, ci kub ntev 80-140, ci sij hawm 2-4 teev.
16. Pei: Nozzle 300-320 degree, pwm kub 180-200 degree, cov khoom kub 120-140 degree, ci sij hawm 2-4 teev.
17. Peek: Nozzle 310-360 degree, pwm kub ua 120-160 degree, cov khoom kub 120-140 degree, ci sij hawm 2-4 teev.
18. PA46: Nozzle 290-300 Degree, pwm kub 80-120 degree, cov khoom kub 290-300℃sijhawm 2-4 teev.